Product Name: | Boiler Tube | Standard: | ASTM A312, ASTM A213, ASTM A269, ASTM A450 |
---|---|---|---|
Material Grade: | TP304/304L, TP310/310S, TP316/316L, TP316Ti, TP317/317L, TP321/321H, TP347/347H | Type: | Seamless / ERW / EFW |
Form: | U-bend, Straight. | NDT: | ET, UT, HT, PT |
Final Finishing: | Solution Annealed & Pickled/Bright Annealed | Application: | Boiler, Heat Exchanger |
High Light: |
TP317L Seamless Tube,ASTM SA213 Seamless Tube,100% ET Boiler Tube |
STANDARD | UNS | WERKSTOFF NR. |
SS 317 | S31700 | 1.4449 |
SS 317L | S31703 | 1.4438 |
Density | 8.0 g/cm3 |
Melting Point | 1454 °C (2650 °F) |
Tensile Strength | Psi - 75000, MPa - 515 |
Yield Strength (0.2%Offset) | Psi - 30000, MPa - 205 |
Elongation | 35 % |
Specific Heat (0-100°C) | Thermal Conductivity | Thermal Expansion | Modulus Elasticity | Electrical Resistivity | Density |
500 | 14.6 | 16.5 | 193 | 7.4 | 7.99 |
J.kg-1.°K-1 | W.m -1.°K-1 | mm/m/°C | GPa | μohm/cm | g/cm3 |
Production | Outside Diameter | Wall Thickness |
BoilerTube | 3.00mm to 219.1mm | 0.4mm to 12.7mm |
Corrosion Test | Conducted only when specially requested by the client |
Chemical Analysis | Test done as per required quality standards |
Destructive / Mechanical Testing | Tensile | Hardness | Flattening | Flare | Flange |
Reverse-bend and Re. flat tests | Carried out in full compliance with relevant standards & ASTM A-450 and A-530 norms, which ensures trouble-free expansion, welding & use at customers end |
Eddy Current Testing | Done to detect homogeneities in subsurface by using Digital Flaw-mark Testing System |
Hydrostatic Testing | 100% Hydrostatic Testing carried out according to ASTM-A 450 norms for checking tube leakage, and biggest pressure we can support 20Mpa/7s . |
Air Under Pressure Test | To check any evidence of air leakage |
Visual Inspection | After passivation, every single length of tubes & pipes is subjected to thorough visual inspection by trained staff for detecting surface flaws & other imperfections |
|
|
|